Yuhong Holding Group Co.,LTD
Hardness and tensile tests measure strength and ductility under slow, steady loading; they do not tell you how a material behaves when struck. The Charpy impact test fills that gap: a notched specimen is broken by a single blow from a pendulum, and the energy absorbed is a measure of toughness. For low-temperature, high-strain-rate or welded service, the impact result can decide whether the grade is acceptable.
A pendulum of known weight is raised to a defined height and released. It strikes a notched specimen supported as a simple beam and breaks it, then swings to a lower height on the other side. The energy absorbed by the specimen is calculated from the difference between the initial and final heights: Ak = 9.8 × G × (H₁ − H₂) J, where G is the pendulum weight and H₁, H₂ the initial and final heights.
The notch concentrates stress and controls where the specimen breaks. Three notch types are standardised:
The notch geometry changes the stress concentration and the deformed volume before fracture. V-notch and U-notch specimens give different absorbed energies for the same material, so the notch type must be stated with the result; a value without it cannot be compared with another impact result.
The Charpy V-notch geometry is standardised internationally, but the pendulum striker radius is defined by the test standard — ASTM A370 specifies 8 mm — and this affects the measured energy. Impact values from different laboratories must therefore be compared with the test standard in view.
The standard test is at room temperature (typically 10–35°C, or 20 ± 2°C where a tighter condition is specified). Where stainless steel is used at low temperature, the test is run at the service temperature: the specimen is cooled in a bath to that temperature, held until uniform, and broken immediately after removal.
Impact energy falls as temperature falls. For austenitic stainless steels, which retain toughness to cryogenic temperatures, the low-temperature impact result is often used to qualify the grade for LNG, cryogenic or cold-climate service. For ferritic and martensitic grades the ductile-to-brittle transition temperature is the critical parameter, and the test is used to locate it.
Two other measures are used alongside the absorbed energy:
The most common impact-test problem we see is a room-temperature value offered for a low-temperature duty — the number looks acceptable, but it was measured at the wrong temperature. For low-temperature and cryogenic projects, we run the test at the service temperature stated in the purchase order and report the notch type, temperature and absorbed energy with the specimen orientation and heat number.
What is the difference between a Charpy V-notch and U-notch test?
The notch geometry changes the stress concentration and the energy absorbed in fracture. V-notch and U-notch specimens give different absorbed energies for the same material, so the notch type must be stated with the result; results from different notch types are not interchangeable.
Why does the test temperature matter for stainless steel?
Impact energy falls as temperature falls. Austenitic stainless steels retain toughness to cryogenic temperatures, while ferritic and martensitic grades show a ductile-to-brittle transition. The test must be run at the service temperature where low-temperature toughness is required.
What does lateral expansion mean in a Charpy test?
Lateral expansion is the amount the specimen expands sideways at the fracture. A larger lateral expansion indicates a tougher material and is reported with the absorbed energy where required.
Can impact results from different laboratories be compared directly?
Only if the notch type, test temperature and test standard are the same. The pendulum striker radius is defined by the test standard — ASTM A370 specifies 8 mm — and this affects the measured energy.
![]()
Contact Person: Mr. Jikin Cai
Tel: +86-13819835483
Fax: 0086-574-88017980