| Standard: | ASTM A789 | Grade: | UNS S32205 |
|---|---|---|---|
| Material: | Duplex Stainless Steel | Outside Diameter: | 1/8"-48" |
| Wall Thickness: | SCH5S To SCHXXS | Types: | Seamless |
| End: | BE/PE | Length: | 6m, 12m, Or As Required |
ASTM A789 UNS S32205 Duplex Steel Tube 450MPa Yield Cl⁻ Resistant for Heat Exchanger
| Chemical Composition – UNS S32205 vs UNS S31803 | ||
| Element | S32205 Range (%) | S31803 Range (%) |
| C (Carbon) | ≤ 0.03 | ≤ 0.03 |
| Mn (Manganese) | ≤ 2.00 | ≤ 2.00 |
| Si (Silicon) | ≤ 1.00 | ≤ 1.00 |
| P (Phosphorus) | ≤ 0.03 | ≤ 0.03 |
| S (Sulfur) | ≤ 0.02 | ≤ 0.02 |
| Cr (Chromium) | 22.0 – 23.0 | 21.0 – 23.0 |
| Ni (Nickel) | 4.5 – 6.5 | 4.5 – 6.5 |
| Mo (Molybdenum) | 3.0 – 3.5 | 2.5 – 3.5 |
| N (Nitrogen) | 0.14 – 0.20 | 0.08 – 0.20 |
| Cu (Copper) | — |
≤ 1.0 (optional) |
| Mechanical Properties – Standard Minimum vs. Typical Values | ||
| Property | ASTM A789 Requirement (Min.) | Typical Value |
| Tensile Strength (Rm) | ≥ 655 MPa (95 ksi) | 825 – 1035 MPa |
| Yield Strength (Rp0.2) | ≥ 450 MPa (65 ksi) | ~550 – 620 MPa |
| Elongation (50mm gage length) | ≥ 25% | 30 – 35% |
| Hardness | ≤ 293 HBW / ≤ 32 HRC | ~19 HRC |
| Physical Properties | ||
| Property | Value | Unit |
| Density | 7.82 – 7.85 | g/cm³ |
| Elastic Modulus (20°C) | 190 – 200 | GPa |
| Thermal Conductivity (100°C) | ~19 | W/(m·K) |
| Coefficient of Linear Expansion (0-100°C) | 13.7 | ×10⁻⁶/°C |
| Electrical Resistivity | ~850 | nΩ·m |
| Melting Range | 1400 – 1455 | °C |
| Heat Treatment Requirements | |
| Item | Requirement |
| Solution Annealing Temperature | 1020°C – 1100°C |
| Cooling Method | Rapid cooling (water quench or rapid air cool) |
| Hardening Method | Cannot be hardened by heat treatment |
| Work Hardening | Cold working produces significant hardening |