Yuhong Holding Group Co.,LTD
| Place of Origin: | CHINA |
| Brand Name: | YUHONG |
| Certification: | ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008 |
| Model Number: | EXTRUDED FIN TUBE |
| Minimum Order Quantity: | 10PCS |
|---|---|
| Price: | Negotiable |
| Packaging Details: | IRON FRAME WOODEN CASE |
| Delivery Time: | Depends on quantity |
| Payment Terms: | L/C,T/T |
| Supply Ability: | 1000 tons per month |
| Base Tube Material: | ASTM A179 Carbon Steel | Fin Material: | AL1060 Aluminum |
|---|---|---|---|
| Fin Attachment Method: | Extruded | Fin Density (FPI): | 5-11 Fins Per Inch |
| Operating Temp Range: | 280°C To 300°C | Typical Application: | HRSG Economizers, Air Coolers |
Extruded Finned Tubes: ASTM A179 Carbon Steel Base with AL1060 Aluminum Fins | High-Efficiency Heat Transfer
Our extruded finned tubes integrate ASTM A179 seamless carbon steel base tubes with high-purity AL1060 aluminum
fins through a hot extrusion process. This creates a metallurgical bond that maximizes thermal conductivity (159 W/m·K
for Al) while maintaining structural integrity under high-pressure environments.
| Parameter | Base Tube (ASTM A179) | Fins (AL1060) |
|---|---|---|
| Outer Diameter | ±0.10 mm | Fin Height: ±0.15 mm |
| Wall Thickness | ±10% | Fin Density: ±1 fin/ft |
| Length | +3/-0 mm | Fin Thickness: ±0.05 mm |
| Straightness | ≤1.5 mm/m | Helix Angle: ±1° |
Base Tube Material (ASTM A179):
| Element | C | Mn | P | S | Si |
|---|---|---|---|---|---|
| Wt. % | ≤0.06-0.18 | 0.27-0.63 | ≤0.035 | ≤0.035 | ≥0.13-0.35 |
Fin Material (AL1060):
| Element | Al | Fe+Si | Cu | Zn | Others |
|---|---|---|---|---|---|
| Wt. % | ≥99.60% | ≤0.35% | ≤0.05% | ≤0.05% | ≤0.03% |
• Heat Recovery Steam Generators (HRSGs)
• Economizers & Air Preheaters (operating temp: 150-400°C)
• Chiller bundles with refrigerant R134a/R410A
• Air-cooled condensers (ambient temp: -40°C to +50°C)
• Waste heat recovery units (flue gas corrosion resistance)
• Petrochemical reactor cooling jackets
• Biomass boiler superheaters
• Geothermal brine heat exchangers
Fin efficiency >92% at 250°C due to extrusion bonding (vs. 70-85% in L-footed tubes)
Withstands 6.9 MPa operating pressure (ASTM A179 yield strength: 180 MPa min)
Al₂O₃ layer formation on fins (thickness: 2-3 nm) prevents acid dew point corrosion
Fin density: 5-11 FPI (fins per inch) | Base tube OD: 15.88 - 50.8 mm
![]()
Contact Person: Freya
Tel: +8617276485535
Fax: 0086-574-88017980